Hardness Conversions for Steels
-
Published:2000
Abstract
Hardness conversions are empirical relationships defined by conversion tables limited to specific categories of materials. This article is a collection of tables that present approximate Rockwell B hardness conversion numbers for nonaustenitic steels as per ASTM E 140 and approximate equivalent hardness numbers for the Brinell hardness and the Vickers (diamond pyramid) hardness numbers for steel.
You do not currently have access to this chapter.
Citation
Hardness Conversions for Steels, Mechanical Testing and Evaluation, Vol 8, ASM Handbook, Edited By Howard Kuhn, Dana Medlin, ASM International, 2000, p 282–287, https://doi.org/10.31399/asm.hb.v08.a0003278
Download citation file:
Related Book Content
Steel Hardness Conversions
Metalworking: Bulk Forming
Steel Hardness Conversions
Heat Treating of Irons and Steels
Steel Hardness Conversions
Metalworking: Sheet Forming
Approximate Equivalent Hardness Numbers and Tensile Strengths for Brinell Hardness Numbers for Steel
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Approximate Equivalent Hardness Numbers and Tensile Strengths for Rockwell C and B Hardness Numbers for Steel
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Approximate Equivalent Hardness Numbers and Tensile Strengths for Vickers Hardness Numbers for Steel
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Growth Curves
Aluminum Alloy Castings Properties, Processes, and Applications
Brittle Fracture of Alloy Steel Chain Links Because of Excessive Hardness
ASM Failure Analysis Case Histories: Material Handling Equipment
Nonferrous Hardness Conversions
Metalworking: Bulk Forming
Fatigue Fracture of a Cast Chromium-Molybdenum Steel Pinion
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment