Corrosion: Fundamentals, Testing, and Protection
Microbiologically Influenced Corrosion Testing
-
Published:2003
Abstract
Corrosion resulting from the presence and activities of microbes on metals and metal alloys is generally referred to as microbiologically influenced corrosion (MIC). This article describes the biofilm formation and structure and microbial processes influencing corrosion. It also discusses the electrochemical techniques used to study and monitor MIC and presents examples of their applications to MIC.
Sign in
ASM members
Member Sign InB.J. Little, F.B. Mansfeld, P.J. Arps, J.C. Earthman, Microbiologically Influenced Corrosion Testing, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 478–486, https://doi.org/10.31399/asm.hb.v13a.a0003647
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.