Corrosion: Fundamentals, Testing, and Protection
Designing to Minimize Corrosion
-
Published:2003
Abstract
Unexpected and frequently costly failures occur due to the lack of sound and reliable engineering design. Therefore, designing against corrosion is essential for reducing such failures. This article provides a discussion on design considerations and general corrosion awareness. It details the functional requirements, such as design and materials selection, which assist in controlling corrosion in different environments. The article also illustrates the design factors that accelerate corrosion.
Peter Elliott, Designing to Minimize Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 929–939, https://doi.org/10.31399/asm.hb.v13a.a0003703
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.