Introduction to Corrosion Resistance of Bulk Materials
By
Paul Natishan
Naval Research Laboratory
Paul Natishan
Search for other works by this author on:
-
Published:2003
Abstract
This article discusses factors that influence the effect of alloying, metallurgical treatments, and mechanical treatments on the corrosion resistance of metallic materials, with schematic illustrations.
Topics
Corrosion,
Environmentally induced corrosion,
Localized corrosion,
Microbiologically-influenced corrosion,
Mechanically assisted corrosion,
Metallurgically influenced corrosion,
Corrosion inhibitors,
Corrosion testing,
Surface treatment,
Ferrous metals and alloys,
Nonferrous metals and alloys
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Paul Natishan, Introduction to Corrosion Resistance of Bulk Materials, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 687–688, https://doi.org/10.31399/asm.hb.v13a.a0003673
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Introduction to Corrosion Resistance of Bulk Materials
Corrosion in the Petrochemical Industry (Second Edition)
Corrosion
Titanium Physical Metallurgy, Processing, and Applications
Stainless Steels
Steels: Processing, Structure, and Performance (Second Edition)
Tensile Testing
Inspection of Metals Understanding the Basics
Principles of Alloying
Alloying Understanding the Basics
Creep and Stress-Rupture Failures
Failure Analysis and Prevention (2021 Edition)
Periodic System for Ferrous Metallurgists
Fundamentals of Modeling for Metals Processing
Low-Expansion Alloys
Alloying Understanding the Basics
Magnetic Alloys
Alloying Understanding the Basics
Stress Relaxation Testing
Mechanical Testing and Evaluation