Gaseous Corrosion-Wear Interactions
By
Joseph H. Tylczak
;
Joseph H. Tylczak
Albany Research Center, U.S. Department of Energy
Search for other works by this author on:
Thomas A. Adler
Thomas A. Adler
Albany Research Center, U.S. Department of Energy
Search for other works by this author on:
-
Published:2003
Abstract
This article provides a discussion on the mechanisms of wear and their interactions with gaseous corrosion. The wear mechanisms include abrasive, erosive, fretting, and sliding. The measurement of degradation on combustion walls in coal-fired boilers is discussed. The article concludes with information on the common coating techniques used for wear-corrosion control.
You do not currently have access to this chapter.
Citation
Joseph H. Tylczak, Thomas A. Adler, Gaseous Corrosion-Wear Interactions, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 338–344, https://doi.org/10.31399/asm.hb.v13a.a0003630
Download citation file:
Related Book Content
Introduction to the Fundamentals of Corrosion
Corrosion: Fundamentals, Testing, and Protection
Methods for Measuring Gaseous Corrosion Rates
Corrosion: Fundamentals, Testing, and Protection
Fatigue Fracture of a D-6ac Steel Structural Member at the Line of Contact With Another Member
ASM Failure Analysis Case Histories: Design Flaws
Fretting Failure of Raceways on 52100 Steel Rings of an Automotive Front- Wheel Bearing
ASM Failure Analysis Case Histories: Automobiles and Trucks
Automotive Proving Ground Corrosion Testing
Corrosion: Environments and Industries
Corrosion in Supercritical Water—Waste Destruction Environments
Corrosion: Environments and Industries
Simulation of Diffusion in Surface and Interface Reactions
Metals Process Simulation
Failures of Mechanical Fasteners
Analysis and Prevention of Component and Equipment Failures
Petroleum Reactor Pressure-Vessel Materials for Hydrogen Service
Damage Mechanisms and Life Assessment of High-Temperature Components
Thermodynamics of Gaseous Corrosion
Corrosion: Fundamentals, Testing, and Protection