Corrosion Rate Conversion
-
Published:2003
Abstract
This article contains a corrosion rate conversion table and a figure that shows the relationships among some of the units commonly used for corrosion rates of metals.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Corrosion Rate Conversion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 1028, https://doi.org/10.31399/asm.hb.v13a.a0003717
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Corrosion Rate Conversion
Corrosion: Environments and Industries
Corrosion Rate Conversion
Corrosion in the Petrochemical Industry (Second Edition)
Basic Concepts Important to Corrosion
Corrosion: Understanding the Basics
Corrosion Rate Conversion
Corrosion: Materials
Corrosion Data
Titanium: A Technical Guide (Second Edition)
Etchants for Revealing Macrostructure
Metallography Principles and Practice
Attack Polishing Procedures
Metallography Principles and Practice
Chemical Polishing Solutions
Metallography Principles and Practice
Description of Hardness Code and Specification of Hardness Numbers for Metals
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Types of Corrosive Environments
Corrosion of Aluminum and Aluminum Alloys