Corrosion: Fundamentals, Testing, and Protection
Statistics for the Corrosionist
-
Published:2003
Abstract
This article presents definitions, equations, and notational conventions that are used widely in statistical analysis. It provides information on a basic framework for the selection of a statistical test. The article outlines the basic elements common to all statistical tests. Illustrations of specific statistical tests and the concept of confidence limits are introduced. The article provides an overview of sampling issues, with guidance on both selecting a sampling method and determining the number of units to sample. One-way analysis of the variance, correlation, and simple regression are also illustrated.
Sign in
ASM members
Member Sign InBarnie P. Jones, Statistics for the Corrosionist, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 972–979, https://doi.org/10.31399/asm.hb.v13a.a0003712
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.