Corrosion: Fundamentals, Testing, and Protection
Anodic Protection
-
Published:2003
Abstract
This article presents a brief history and the uses of the anodic protection technique. It compares anodic and cathodic protection and describes the design considerations of the anodic protection system. The article discusses the specific requirements of equipment required for anodic protection. It also explains the applications and economic aspects of anodic protection, with examples.