Corrosion: Fundamentals, Testing, and Protection
Effects of Metallurgical Variables on the Corrosion of Stainless Steels
-
Published:2003
Abstract
Metallurgical variables, mainly carbon distribution and the presence of nitrogen and metallic phases, can influence the corrosion behavior of austenitic, ferritic, duplex, and martensitic stainless steels. This article describes the effects of these metallurgical and processing variables on the susceptibility of the stainless steels to intergranular corrosion and intergranular stress-corrosion cracking and their testing methods. It explains the effect of sigma and related phases on the corrosion behavior of stainless steels.
Sign in
ASM members
Member Sign InJames D. Fritz, Effects of Metallurgical Variables on the Corrosion of Stainless Steels, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 266–274, https://doi.org/10.31399/asm.hb.v13a.a0003617
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.