Corrosion: Fundamentals, Testing, and Protection
Introduction to Corrosion for Constructive Purposes
-
Published:2003
Abstract
Principles of metallic corrosion play a fundamental role in developing industrial processes that employ corrosion for constructive purposes. This article examines the changes in kinetics that occur with differentially small potential changes around the equilibrium electrode potentials of two reversible electrodes, such as copper and silver electrodes, in an electrochemical system. It provides a schematic illustration of a reversible cell with copper and silver electrodes to determine a reversible cell potential between the electrodes. An electrode becomes irreversible when the electrode reactions are displaced from equilibrium and the electrode potential is no longer at the equilibrium potential. The article...
Sign in
ASM members
Member Sign InMałgorzata Ziomek-Moroz, Introduction to Corrosion for Constructive Purposes, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 135–138, https://doi.org/10.31399/asm.hb.v13a.a0003604
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.