Abstract
The corrosion behavior of a metal or alloy is determined by its composition and structural features, the environment and stresses to which it is exposed, and the behavior of any corrosion products generated. This article provides a detailed discussion on the fundamentals of pure metals, impure metals, and alloys. It highlights the ways in which the metallurgical variables, namely, composition and structure, influence the corrosion properties of metals and alloys in aqueous environment.
Sign in
ASM members
Member Sign InJames J. Noël, Effects of Metallurgical Variables on Aqueous Corrosion, Corrosion: Fundamentals, Testing, and Protection, Vol 13A, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2003, p 258–265, https://doi.org/10.31399/asm.hb.v13a.a0003616
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!