Grit Sizes and Grain Size Conversions
-
Published:2004
Abstract
This article contains a conversion table, which assists in the conversion of ASTM number to average grain intercept length. It also includes a table that lists European and U.S. grit numbers with their approximate particle size for metallographic grinding papers.
You do not currently have access to this chapter.
Citation
Grit Sizes and Grain Size Conversions, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, p 1093, https://doi.org/10.31399/asm.hb.v09.a0003726
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.
Related Book Content
The Relationship between the ASTM Grain Size and the Average “Diameter” of the Grain
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Quantitative Metallography
Materials Characterization (2019 Edition)
Austenitization
Light Microscopy of Carbon Steels
Measurement of Microstructure
Metals Handbook Desk Edition (2nd Edition)
Classification of Carbon and Low-Alloy Steels
Practical Heat Treating Basic Principles
Heat Treating of Magnesium Alloys
Heat Treating of Nonferrous Alloys
Neutron Diffraction
Materials Characterization
Heat Treating Basics
Practical Induction Heat Treating (Second Edition)
Fracture of a Cast Stainless Steel Femoral Prosthesis
Handbook of Case Histories in Failure Analysis
An Investigative Analysis of the Properties of Severely Segregated A441 Bridge Steel
ASM Failure Analysis Case Histories: Buildings, Bridges, and Infrastructure