Special Sample Preparation and Polishing for Fiber-Reinforced Composites[1]
-
Published:2004
Abstract
This article focuses on the sample preparation methods for titanium honeycomb composites, boron fiber composites, and titanium/polymeric composite hybrids. These include mounting, sectioning, grinding, and polishing. The article also provides information on the sample preparation of unstaged and staged prepreg materials for optical analysis.
Brian S. Hayes, Luther M. Gammon, Special Sample Preparation and Polishing for Fiber-Reinforced Composites, Metallography and Microstructures, Vol 9, ASM Handbook, Edited By George F. Vander Voort, ASM International, 2004, https://doi.org/10.31399/asm.hb.v09.a0009074