Ternary Alloy Phase Diagrams
-
Published:2016
Abstract
This article presents ternary alloy phase diagrams to be used primarily by engineers to solve industrial problems. The diagrams presented are for stable equilibrium conditions, with the exception of metastable conditions for some diagrams involving carbon and iron. In some ternary diagrams involving carbon and iron, the symbol M is used to represent both iron and the other metallic element when the two metals substitute for each other in a carbide phase.
You do not currently have access to this chapter.
Citation
Ternary Alloy Phase Diagrams, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 643, https://doi.org/10.31399/asm.hb.v03.a0006246
Download citation file:
Related Book Content
Microstructures of Nitrided Iron and Steel
Practical Nitriding and Ferritic Nitrocarburizing
Fundamentals of Steel Heat Treatment
Practical Heat Treating Basic Principles
Specifications and Selection of Gray Irons
Cast Iron Science and Technology
Glossary of Terms: Surface Engineering
Surface Engineering
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice
Introduction to Steels and Cast Irons
Metallographer’s Guide Practices and Procedures for Irons and Steels
Glossary
Metallographer’s Guide Practices and Procedures for Irons and Steels
Periodic System for Ferrous Metallurgists
Fundamentals of Modeling for Metals Processing
High-Temperature Combustion
Materials Characterization
Carbon Arc Welding
Welding, Brazing, and Soldering