Ag (Silver) Ternary Alloy Phase Diagrams
-
Published:2016
Abstract
This article is a compilation of ternary alloy phase diagrams for which silver (Ag) is the first-named element in the ternary system. The diagrams are presented with element compositions in weight percent. The article includes 16 phase diagrams: Ag-Au-Cu liquidus projection; Ag-Au-Cu isothermal section at 850 °C; Ag-Au-Cu isothermal section at 950 °C; Ag-Au-Cu isothermal section at 775 °C; Ag-Au-Cu isothermal section at 300 °C; Ag-Cd-Cu isothermal section at 600 °C; Ag-Cd-Cu liquidus projection; Ag-Cd-Cu isothermal section at 500 °C; Ag-Cd-Cu isothermal section at 300 °C; Ag-Cd-Zn isothermal section at 600 °C; Ag-Cd-Zn liquidus projection; Ag-Cd-Zn isothermal section at 400 °C; Ag-Cd-Zn isothermal section at 200 °C; Ag-Cu-Zn isothermal section at 600 °C; Ag-Cu-Zn liquidus projection; and Ag-Cu-Zn isothermal section at 350 °C.
Ag (Silver) Ternary Alloy Phase Diagrams, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 644–647, https://doi.org/10.31399/asm.hb.v03.a0006232
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!