Alloy Phase Diagrams
Solid Solutions and Phase Transformations[1]
-
Published:2016
Abstract
This article begins with the one-component, or unary, diagram for magnesium. The diagram shows what phases are present as a function of the temperature and pressure. When two metals are mixed in the liquid state to produce a solution, the resulting alloy is called a binary alloy. The article describes the various types of solid solutions such as interstitial solid solutions and substitutional solid solutions. Free energy is important because it determines whether or not a phase transformation is thermodynamically possible. The article discusses the thermodynamics of phase transformations and free energy, as well as kinetics of phase transformations....
Sign in
ASM members
Member Sign InSolid Solutions and Phase Transformations, Alloy Phase Diagrams, Vol 3, ASM Handbook, Edited By H. Okamoto, M.E. Schlesinger, E.M. Mueller, ASM International, 2016, p 17–25, https://doi.org/10.31399/asm.hb.v03.a0006222
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!