Abrasive Waterjet Cutting
-
Published:2006
Abstract
This article provides a detailed account of the process development, cutting principle, and components of the abrasive waterjet cutting process. The advantages of abrasive waterjet machining are summarized. The article also discusses the factors affecting the cut quality, and the applications and limitations of abrasive waterjet cutting.
Topics
Abrasive waterjet cutting
You do not currently have access to this chapter.
Citation
Abrasive Waterjet Cutting, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 120–129, https://doi.org/10.31399/asm.hb.v14b.a0005107
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Machining
Titanium: A Technical Guide (Second Edition)
Cutting Operations
Metalworking: Sheet Forming
2011 and 2012 Free Machining Aluminum Alloy
Properties and Selection of Aluminum Alloys
Waterjet/Abrasive Waterjet Machining
Machining
Machining of Carbon and Alloy Steels
Machining
Microstructure and Machinability
Metals Handbook Desk Edition (2nd Edition)
Elements of the Machining Process
Metals Handbook Desk Edition (2nd Edition)
Laser Cutting, Drilling, and Shock Peening
Welding Fundamentals and Processes
Metal Removal
Schey’s Tribology in Metalworking Friction, Lubrication, and Wear