Abstract
This article discusses the advantages and limitations of drop hammer forming and presents the key factors for determining a process plan. It describes the characteristics of hammers and presents information on tool materials. It explains the use of lubricants and preparation of blanks for forming. The article also details the drop hammer forming process of steels, aluminum alloys, magnesium alloys, and titanium alloys.
You do not currently have access to this chapter.
Citation
Drop Hammer Forming, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 419–423, https://doi.org/10.31399/asm.hb.v14b.a0005128
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Fatigue and Fracture of Engineering Alloys
Fatigue and Fracture Understanding the Basics
Heat Treatment of Nonferrous Alloys
Metallurgy for the Non-Metallurgist (Second Edition)
Heat Treating of Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)
Heat Treatment of Aluminum and Other Nonferrous Alloys
Practical Heat Treating Basic Principles
Forming of Titanium Plate, Sheet, Strip, and Tubing
Titanium Physical Metallurgy, Processing, and Applications
Forming of Magnesium Alloys
Metalworking: Sheet Forming
Heat Treatable Nonferrous Alloys
Heat Treating of Nonferrous Alloys
Forging of Specific Metals and Alloys
Metals Handbook Desk Edition (2nd Edition)
Arc Welding
Metals Handbook Desk Edition (2nd Edition)
Foundry Practice for Nonferrous Alloys
Metals Handbook Desk Edition (2nd Edition)