Abstract
This article focuses on the mechanical and nonmechanical cutting methods used in metal fabrication industries. The most prevalent equipment used for mechanical cutting includes shears, iron workers, nibblers, and band saws. Nonmechanical methods of cutting include gas cutting, electric arc cutting, and laser cutting. The article concludes with information on the advantages of abrasive waterjet cutting, which is an alternative to laser cutting, gas cutting, and plasma cutting.
Cutting Operations, Metalworking: Sheet Forming, Vol 14B, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2006, p 23–27, https://doi.org/10.31399/asm.hb.v14b.a0005174