Abstract
This article provides information on fracture toughness and fatigue crack growth of structural steels. It describes fatigue life behavior in terms of unnotched fatigue limits, notch effects, axial strain-life fatigue, and mean stress effects. The article analyzes the mechanisms of corrosion fatigue crack initiation and prevention of corrosion fatigue. It presents case histories of fatigue failure of various steel components. The article reviews the failure of coiled tubing in a drilling application and the failure of coiled tubing due to hydrogen sulfide exposure, with examples.
Alexander D. Wilson, Fracture and Fatigue Properties of Structural Steels, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 591–604, https://doi.org/10.31399/asm.hb.v19.a0002395
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.