Fatigue and Fracture
Fatigue Crack Growth under Variable-Amplitude Loading
-
Published:1996
Abstract
This article summarizes fatigue phenomena in metallic materials. It discusses fatigue under variable-amplitude (VA) loading, with emphasis on crack growth. The article presents the prediction models of crack initiation and crack growth under VA loading. It concludes with a discussion on the conditions associated with engineering applications of VA loading.
J. Schijve, Fatigue Crack Growth under Variable-Amplitude Loading, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 110–133, https://doi.org/10.31399/asm.hb.v19.a0002356