Fatigue and Fracture
Fatigue Properties in Engineering
-
Published:1996
Abstract
Fatigue properties are an integral part of materials comparison activities and offer information for structural life estimation in many engineering applications. This article presents three general approaches to fatigue design, with a discussion on their respective attributes. These include infinite-life criterion, finite-life criterion, and damage tolerant criterion. The article describes the individual property requirements of these approaches. It also presents selected examples of properties that reflect some detail of these approaches.
Sign in
ASM members
Member Sign InD.W. Cameron, D.W. Hoeppner, Fatigue Properties in Engineering, Fatigue and Fracture, Vol 19, ASM Handbook, By ASM Handbook Committee, ASM International, 1996, p 15–26, https://doi.org/10.31399/asm.hb.v19.a0002350
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!