Metalworking: Bulk Forming
Roll Forming of Axially Symmetric Components
-
Published:2005
Abstract
This article describes the roll forming of components of nickel, titanium, and aluminum alloys. The metallurgical characteristics of the roll formed components, such as macrostructures, microstructures, tensile strength, and stress rupture performance, are discussed. The article compares the resulting properties of roll formed and conventionally forged components.
Sign in
ASM members
Member Sign InB.P. Bewlay, M.F.X. Gigliotti, C.U. Hardwick, O.A. Kaibyshev, V.A. Valitov, D.U. Furrer, Roll Forming of Axially Symmetric Components, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 480–488, https://doi.org/10.31399/asm.hb.v14a.a0004010