Roll Forging
By
Prabir K. Chaudhury
;
Prabir K. Chaudhury
Orbital Sciences Corporation
Search for other works by this author on:
Roger Rees
Roger Rees
Forging Division, SMS Eumuco Inc.
Search for other works by this author on:
-
Published:2005
Abstract
Roll forging is a process for simultaneously reducing the cross-sectional area and changing the shape of heated bars, billets, or plates. This article provides an overview of the process capabilities, production techniques, machines and machine size selection considerations, and types of roll dies and auxiliary tools for the roll forging. It concludes with information on the production examples of roll forging.
You do not currently have access to this chapter.
Citation
Prabir K. Chaudhury, Roger Rees, Roll Forging, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 131–135, https://doi.org/10.31399/asm.hb.v14a.a0003981
Download citation file:
Related Book Content
Billet Separation and Shearing
Cold and Hot Forging Fundamentals and Applications
Forging of Aluminum Alloys
Aluminum Science and Technology
Billet Casting Principles and Practice
Aluminum Extrusion Technology
Extrusion of Hard Alloys
Aluminum Extrusion Technology
Practical Aspects of Converting Ingot to Billet
Metalworking: Bulk Forming
Machinery and Equipment for Direct and Indirect Hot Extrusion
Extrusion (Second Edition)
Ingot Metallurgy and Mill Products
Titanium: A Technical Guide (Second Edition)
Alclad 2029 High-Strength, High-Toughness Sheet/Plate
Properties and Selection of Aluminum Alloys
Ultrasonic Inspection of a 1.7 m (68 in.) Diam 8822 Steel Billet and the Ring Into Which It Was Rolled
ASM Failure Analysis Case Histories: Processing Errors and Defects
Metallurgical Principles
Extrusion (Second Edition)