The distinction between an unconfined web and a confined web describes the relative ease of flow of metal to flash during forging. This article describes the various types of unconfined and confined web-and-rib combinations encountered in the design of forgings. It informs that the limits suggested by forging producers and users covering minimum web thicknesses that are producible are helpful in estimating the producibility of a given web thickness in projected-forging design. The article briefly analyzes the web designs of several forgings, including designs for producing flat webs, contoured webs, and oblique webs. It provides a checklist to be reviewed by a web designer.
Forging Design Involving Webs, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 775–792, https://doi.org/10.31399/asm.hb.v14a.a0004039
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!