Abstract
This article reviews the general aspects of product design and provides an overview of the manufacturing processes and their relationship to design, with an emphasis on deformation processes. It discusses the various classes of deformation processes to illustrate their impacts on product design while taking advantage of the benefits of deformation processing.
You do not currently have access to this chapter.
Citation
Howard Kuhn, Design for Deformation Processing, Metalworking: Bulk Forming, Vol 14A, ASM Handbook, Edited By S.L. Semiatin, ASM International, 2005, p 11–20, https://doi.org/10.31399/asm.hb.v14a.a0003972
Download citation file:
Related Book Content
Manufacturing Cost Estimating
Metals Process Simulation
Failure Causes
Composites
Metal Forming Processes in Manufacturing
Cold and Hot Forging Fundamentals and Applications
Dimensional Management and Tolerance Analysis
Materials Selection and Design
Why Perform Failure Analysis?
Understanding How Components Fail (Third Edition)
High-Pressure Die Casting
Casting
Products Liability and Design
Materials Selection and Design
Documenting and Communicating the Design
Materials Selection and Design
Design for Quality
Materials Selection and Design
Cross-Functional Design Teams
Materials Selection and Design