Failures of Locomotive Axles[1]
By
George F. Vander Voort
Carpenter Technology Corporation
George F. Vander Voort
Search for other works by this author on:
-
Published:2002
Abstract
This article provides a background of friction-bearing failures due to overheating. The failures of locomotive axles caused by overheated traction-motor support bearings are discussed. The article also describes liquid-metal embrittlement (LME) in steel. It examines the results of various axle studies, with illustrations and concludes with information on the simulation of the LME mechanism.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
George F. Vander Voort, Failures of Locomotive Axles, Failure Analysis and Prevention, Vol 11, Edited By William T. Becker, Roch J. Shipley, ASM International, 2002, https://doi.org/10.31399/asm.hb.v11.a0001822
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Steel Failures due to Tempering and Isothermal Heat Treatment
Failure Analysis of Heat Treated Steel Components
Metallographic Characterization of Liquid Metal Embrittlement in a Failed Locomotive Axle
ASM Failure Analysis Case Histories: Rail and Rolling Stock
Creep Failure of a 2.25Cr-1Mo Steel Superheater Tube
ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions
Failure of a Pump Shaft Ascribed to Accidental Local Heating
ASM Failure Analysis Case Histories: Chemical Processing Equipment
Failures from Various Mechanisms and Related Environmental Factors
Metals Handbook Desk Edition (2nd Edition)
Examination of an Oxidized Heating Coil
ASM Failure Analysis Case Histories: Steelmaking and Thermal Processing Equipment
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels