Procedure Development and Practice Considerations for Resistance Welding
-
Published:2011
Abstract
This article describes the significance of the three variables that affect the resistance spot welding process: welding current, electrode force, and welding time. It presents the effects of weld spacing and surface preparation on weld quality. The article elaborates the typical sequence of steps for determining the satisfactory conditions for spot welding and the mechanical aspects that affect this process. It considers the effects of process variables on the weld lobe. The article reviews surface preparation, part fit-up, electrode drives, weld parameters, and tests associated with seam welding. It concludes with a discussion on the welding equipment and other...
Sign in
ASM members
Member Sign InMurali D. Tumuluru, Hongyang Zhang, R. (Bob) Matteson, Procedure Development and Practice Considerations for Resistance Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 463–485, https://doi.org/10.31399/asm.hb.v06a.a0005640
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!