High-Frequency Welding[1]
Revising author
-
Published:2011
Abstract
High-frequency resistance welding (HFRW) is a process that uses high-frequency currents to concentrate the welding heat at the desired location. This article focuses on the fundamentals, advantages, limitations, and applications of HFRW. It discusses the personnel and equipment requirements as well as safety considerations necessary for the process. The article concludes with a discussion on the techniques for inspection and quality control of HFRW.
Sign in
ASM members
Member Sign InMenachem Kimchi, High-Frequency Welding, Welding Fundamentals and Processes, Vol 6A, ASM Handbook, Edited By T. Lienert, T. Siewert, S. Babu, V. Acoff, ASM International, 2011, p 456–462, https://doi.org/10.31399/asm.hb.v06a.a0005583