Casting
Abstract
In most castings, there are junctions between intersecting component members. This article describes how defects can be eliminated in five types of junctions in steel castings, namely the L-junction, T-junction, V-junction, X-junction, and Y-junction. It also discusses design considerations for junctions in aluminum castings and provides a comparison between the T-junction and Y-junction. Finally, the article illustrates recommended methods for minimizing defects where sections of unequal thickness form a junction.
Design Problems Involving Junctions, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, https://doi.org/10.31399/asm.hb.v15.a0009024