White Iron and High-Alloyed Iron Castings
By
Richard B. Gundlach
Stork Climax Research Services
Richard B. Gundlach
Search for other works by this author on:
-
Published:2008
Abstract
This article presents a discussion on the melting, pouring, and shakeout practices; composition control; molds, patterns, and casting design; heat treatment; and applications of different classes of nickel-chromium white irons and high-chromium white irons.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
Richard B. Gundlach, White Iron and High-Alloyed Iron Castings, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 896–903, https://doi.org/10.31399/asm.hb.v15.a0005327
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!
Related Book Content
Titanium and Titanium Alloy Castings
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Castability, Product Design, and Production of High-Alloy Iron Castings
Cast Iron Science and Technology
Specification, Selection, and Applications of High-Alloy Iron Castings
Cast Iron Science and Technology
Thin-Wall Gray Iron Castings
Cast Iron Science and Technology
Cast Iron Foundry Practices
Casting
Metallographic Techniques in Failure Analysis
Failure Analysis and Prevention (2021 Edition)
Heat Treating of High-Alloy White Cast Irons
Heat Treating of Irons and Steels
Properties of Titanium-Alloy Welds
Weld Integrity and Performance
Fatigue and Fracture Properties of Aluminum Alloy Castings
Fatigue and Fracture