Vertical Centrifugal Casting[1]
Revising author
-
Published:2008
Abstract
Vertical centrifugal casting machines, installed below the ground level for maximum operator safety, are used for producing bushings and castings that are relatively large in diameter and short in length. This article discusses the mold design for different types of sand molds and permanent molds and their production considerations. It describes the speed of rotation, mold speeds curves, and pouring techniques that are considered in the operation of vertical centrifugal casting machines.
Y.V. Murty, Vertical Centrifugal Casting, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 680–686, https://doi.org/10.31399/asm.hb.v15.a0005259
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.