Abstract
Gravity has profound influences on most solidification and crystal growth processes. Modification of gravity over practical time scales for the purposes of modifying or controlling solidification proves to be a far more daunting and expensive technological challenge. This article discusses various microgravity solidification experiments that involve pure metals, alloys, and semiconductors and presents the official NASA acronyms for them. MEPHISTO, TEMPUS, the isothermal dendritic growth experiment, and advanced gradient heating facility, are also discussed.
Sign in
ASM members
Member Sign InMartin E. Glicksman, Solidification Research in Microgravity, Casting, Vol 15, ASM Handbook, Edited By Srinath Viswanathan, Diran Apelian, Raymond J. Donahue, Babu DasGupta, Michael Gywn, John L. Jorstad, Raymond W. Monroe, Mahi Sahoo, Thomas E. Prucha, Daniel Twarog, ASM International, 2008, p 398–401, https://doi.org/10.31399/asm.hb.v15.a0005228
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!