Corrosion in Marine Atmospheres
-
Published:2006
Abstract
Several factors contribute to marine-atmospheric corrosion with the local environment being the single most important factor. Therefore, assessing a local environment, which is essential to reduce the gross expenditure, is assisted by modeling of the local environment and by a set of corrosion standards proposed by the International Standards Organization (ISO). This article focuses on the important variables associated with atmospheric corrosion in marine atmospheres, namely, moisture, temperature, winds, airborne contaminants, alloy content, location, and biological organisms along with their corresponding assessing methods. It also examines the ISO CORRAG program for modeling the corrosion rate of atmospheric corrosion that...
Sign in
ASM members
Member Sign InRichard B. Griffin, Corrosion in Marine Atmospheres, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 42–60, https://doi.org/10.31399/asm.hb.v13c.a0004106
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.