ASM Handbook
Corrosion: Environments and Industries
ASM International
Volume
13C
ISBN electronic:
978-1-62708-184-9
Publication date:
2006
Abstract
Understanding the high-temperature corrosion behavior of alloys is an important step toward the selection of appropriate alloys for process equipment. This article briefly describes the high-temperature corrosion modes that are frequently encountered in the chemical process industry. These modes include oxidation, carburization, metal dusting, nitridation, halogen corrosion, and sulfidation.
You do not currently have access to this chapter.
Citation
George Y. Lai, Corrosion in High-Temperature Environments, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 754–761, https://doi.org/10.31399/asm.hb.v13c.a0004189
Download citation file:
Related Book Content
Corrosion of Metal Processing Equipment
Corrosion: Environments and Industries
Carburization and Metal Dusting
High-Temperature Corrosion and Materials Applications
High-Temperature Corrosion-Related Failures
Failure Analysis and Prevention
Corrosion of Intermetallics
Corrosion: Materials
Corrosion of Cast Stainless Steels
Corrosion: Materials
High-Temperature Gaseous Corrosion
Corrosion in the Petrochemical Industry (Second Edition)
High-Temperature Gaseous Corrosion
Corrosion: Fundamentals, Testing, and Protection
High-Temperature Corrosion-Related Failures
Failure Analysis and Prevention (2021 Edition)
Gaseous Corrosion Mechanisms
Corrosion: Fundamentals, Testing, and Protection
High-Temperature Gaseous Corrosion Testing
Corrosion: Fundamentals, Testing, and Protection