Abstract
This article provides a detailed discussion on the various devices by which cathodic protection (CP) can be applied to pipe-type power transmission cables. These devices include the resistor rectifier, isolator-surge protector, polarization cells, and field rectifiers. The article describes the interference created by stray currents on CP and associated remedial actions.
Sign in
ASM members
Member Sign InAdrian Santini, Cathodic Protection of Pipe-Type Power Transmission Cables, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 122–125, https://doi.org/10.31399/asm.hb.v13c.a0004118