Corrosion: Environments and Industries
Introduction to Corrosion in Specific Industries
-
Published:2006
Abstract
This article provides a summary of the concepts discussed in the Section “Corrosion in Specific Industries” in the ASM Handbook, Volume 13C:Corrosion: Environments and Industries. This Section applies the fundamental understanding of corrosion and knowledge of materials of construction to practical applications. The industries addressed are nuclear power, fossil and alternative fuel, land transportation, air transportation, microelectronics, chemical processing, pulp and paper, food and beverage, pharmaceutical and medical technology, petroleum and petrochemical, building, and mining and metal processing.
Sign in
ASM members
Member Sign InHira S. Ahluwalia, Introduction to Corrosion in Specific Industries, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 337–338, https://doi.org/10.31399/asm.hb.v13c.a0004144
Download citation file:
2022 ASM International Catalog: Issue 1
View new, upcoming, and best-selling ASM Handbooks, technical books, and databases.