Chemical Cleaning and Cleaning-Related Corrosion of Process Equipment
Revising author
-
Published:2006
Abstract
This article describes the eight chemical cleaning methods, namely, circulation, fill and soak, cascade, foam, vapor-phase organic, steam-injected, on-line chemical, and mechanical cleaning. It presents information on deposit types, solvents used to remove them, and construction material incompatibilities in a table. The article summarizes the uses of chemical cleaning solutions, including hydrochloric acid, phosphoric acid, and sulfamic acid, as well as the additives used to neutralize their impact on corrosion. It discusses the chemical cleaning procedures, including selection of cleaning method and solvent, documentation of cleaning, and corrosion monitoring in chemical cleaning.
Sign in
ASM members
Member Sign InBert Moniz, Jack W. Horvath, Chemical Cleaning and Cleaning-Related Corrosion of Process Equipment, Corrosion: Environments and Industries, Vol 13C, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2006, p 323–330, https://doi.org/10.31399/asm.hb.v13c.a0004143
Download citation file:
2022 ASM International Catalog: Issue 1
View new, upcoming, and best-selling ASM Handbooks, technical books, and databases.