Corrosion: Materials
Corrosion-Resistant Powder Metallurgy Alloys
-
Published:2005
Abstract
This article provides a detailed discussion on the most commonly employed tests and specific examples of the use of these tests in evaluating the corrosion resistance of powder metallurgy (P/M) stainless steels. It describes the influence of various processing parameters on the corrosion resistance of P/M stainless steels. The approaches used to improve the corrosion resistance of sintered stainless steels are discussed briefly. The article also presents a discussion on the manufacturing and corrosion characteristics of P/M superalloys.
Barbara Shaw, Corrosion-Resistant Powder Metallurgy Alloys, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 447–475, https://doi.org/10.31399/asm.hb.v13b.a0003835
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.