Introduction to Environmental Performance of Nonmetallic Materials
By
David C. Silverman
David C. Silverman
Argentum Solutions, Inc.
Search for other works by this author on:
-
Published:2005
Publication history
April 07, 2006
Abstract
This article provides an overview of the environmental performance of the most commonly used nonmetallic materials, including elastomers, plastics, thermosetting resins, resin-matrix composites, organic coatings, concrete, refractories, and ceramics. It also discusses the applications and uses of these materials.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
David C. Silverman, Introduction to Environmental Performance of Nonmetallic Materials, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 545–546, https://doi.org/10.31399/asm.hb.v13b.a0003840
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
Tribology of Plastics and Elastomers
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Property Comparison Tables: Hardness and Tensile Properties
Mechanical Testing and Evaluation
Hardness Measurement of Plastics and Elastomers
Hardness Testing Principles and Applications
Corrosion in Petroleum Production Operations
Corrosion: Environments and Industries
Mechanical Testing and Properties of Plastics: An Introduction
Characterization and Failure Analysis of Plastics
Glossary of Terms: Mechanical Testing and Evaluation
Mechanical Testing and Evaluation
Electrical Testing of Polymers
Engineered Materials Handbook Desk Edition
Materials Issues in Joining
Joining Understanding the Basics
Corrosion in Petroleum Production Operations
Corrosion in the Petrochemical Industry (Second Edition)
Opportunities for Powder-Binder Forming Technologies
Binder and Polymer Assisted Powder Processing