This article, primarily focusing on atmospheric corrosion of carbon and low-alloy steels, describes the factors that must be considered by alloy casting users in material selection. It presents compositions of cast steels tested in atmospheric corrosion in a tabular form. The article graphically presents the results of a research program that compared the corrosion resistance of nine cast steels in marine and industrial atmospheres. It provides a comparison of corrosion rates of cast steels, malleable cast iron, and wrought steel after three years of exposure in two atmospheres. Conclusions drawn from these tests are also presented.