Abstract
This article discusses a tool for the conversion of measurements made against various reference electrodes at different temperatures. It reviews different electrode potential temperature coefficients, namely, isothermal temperature coefficient and thermal temperature coefficient. The article contains a table that lists the electrode potentials and conversion factors for various reference electrodes.
You do not currently have access to this chapter.
Citation
Reference Electrodes, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 662, https://doi.org/10.31399/asm.hb.v13b.a0003799
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!
Related Book Content
Electrochemical Corrosion-Rate Measurements
Fundamentals of Electrochemical Corrosion
Electrogravimetry
Materials Characterization
Potential Measurements with Reference Electrodes
Corrosion: Fundamentals, Testing, and Protection
Effects of Metallurgical Variables on the Corrosion of High-Nickel Alloys
Corrosion: Fundamentals, Testing, and Protection
Molten Salt Corrosion Thermodynamics
Corrosion: Fundamentals, Testing, and Protection
Introduction to Corrosion for Constructive Purposes
Corrosion: Fundamentals, Testing, and Protection
Electrode Potentials
Corrosion: Fundamentals, Testing, and Protection