Corrosion of Hafnium and Hafnium Alloys
-
Published:2005
Abstract
This article describes the processes involved in the production of hafnium and its alloys. It discusses the physical, mechanical and chemical properties of hafnium. The aqueous corrosion testing of hafnium and its alloys is detailed. The article reviews the corrosion resistance of hafnium in specific media, namely, water, steam, hydrochloric acid, nitric acid, sulfuric acid, alkalis, organics, molten metals, and gases. Forms of corrosion, namely, galvanic corrosion, crevice corrosion, and pitting corrosion are included. The article explains the corrosion of hafnium alloys such as hafnium-zirconium alloys and hafnium-tantalum alloys. It also deals with the applications of hafnium and its alloys in the nuclear and chemical industries.
D.R. Holmes, Corrosion of Hafnium and Hafnium Alloys, Corrosion: Materials, Vol 13B, ASM Handbook, Edited By Stephen D. Cramer, Bernard S. Covino, Jr., ASM International, 2005, p 354–359, https://doi.org/10.31399/asm.hb.v13b.a0003826
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!