Abstract
This article reviews various segments of the powder metallurgy (PM) process from powder production and powder processing through the characterization of the materials and their properties. It covers the processing methods for consolidating metal powders including options for processing to full density. The article outlines the freeform fabrication process, also known as additive manufacturing and describes finishing operations of PM parts. It concludes with information on the applications of PM parts.
You do not currently have access to this chapter.
Citation
W. Brian James, Powder Metallurgy Methods and Applications, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 9–19, https://doi.org/10.31399/asm.hb.v07.a0006022
Download citation file:
Related Book Content
History of Powder Metallurgy
Powder Metallurgy
High-Strength Aluminum Powder Metallurgy Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Particle Image Analysis
Powder Metallurgy
Copper P/M Products
Metals Handbook Desk Edition (2nd Edition)
Conventional Powder Metallurgy Aluminum Alloys
Powder Metallurgy
Introduction to Metal Powder Production and Characterization
Powder Metallurgy
Pressed-and-Sintered Ferrous Powder Metallurgy Parts
Metals Handbook Desk Edition (2nd Edition)
High-Temperature Sintering of Ferrous Powder Metallurgy Components
Powder Metallurgy
Modeling and Simulation of Press and Sinter Powder Metallurgy
Powder Metallurgy
A Brief History of the Development of Thermal Spray Processes and Materials
Thermal Spray Technology