Heat Treatment of Secondary-Hardening High-Alloy Tool Steels
-
Published:2015
Abstract
High-potential high-alloy tool steels (HATS) containing martensitic microstructure with undissolved hard phases are achieved by a number of complex heat treating cycles, predominantly tempering. This article focuses on three tempering treatments, namely, salt bath heat treatment, austenitizing, and vacuum heat treatment. It explains the result of these tempering processes with HSS M2 grade of HATS.
Sign in
ASM members
Member Sign InPaul Beiss, Heat Treatment of Secondary-Hardening High-Alloy Tool Steels, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 515–523, https://doi.org/10.31399/asm.hb.v07.a0006128
Download citation file:
Understanding the Basics Collection
8-Volume Digital Library Exclusive
The Understanding the Basics Collection provides comprehensive coverage of critical topics in metallurgy. These introductory guides present critical information on key topics related to materials processing, performance, and evaluation.