Production of Carbide Powders
-
Published:2015
Abstract
This article discusses the methods and procedures used to extract, purify, and synthesize tungsten carbide powder, metal, and other refractory carbide/nitride powders used in hard metal production. Selection of powders, additives, equipment, and processes for making ready-to-press hard metal powders is also discussed. The article also provides information on the emerging technologies for tungsten carbide synthesis and binders in hard metal production, such as cobalt, iron, and nickel.
Sign in
ASM members
Member Sign InThomas A. Wolfe, John L. Johnson, Pankaj K. Mehrotra, Production of Carbide Powders, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 711–714, https://doi.org/10.31399/asm.hb.v07.a0006052