Abstract
Milling of materials, whether hard and brittle or soft and ductile, is of prime interest and of economic importance to the powder metallurgy (PM) industry. This article discusses the principles of milling, milling parameters, and the powder characteristics required for the process. It discusses the changes in powder particle morphology that occur during milling of metal powders produced by various processes such as microforging, fracturing, agglomeration, and deagglomeration. The article also provides useful information on milling equipment such as tumbler ball mills, vibratory ball mills, attrition mills, and hammer and rod mills.
Chris Schade, Milling of Brittle and Ductile Materials, Powder Metallurgy, Vol 7, ASM Handbook, Edited By P. Samal, J. Newkirk, ASM International, 2015, p 77–87, https://doi.org/10.31399/asm.hb.v07.a0006089
Download citation file:
Data Ecosystem
The ASM Data Ecosystem is a new and innovative product line that arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.