This appendix contains sample problems with worked solutions pertaining to the use of binary phase diagrams. The problems require the determination of favorable temperatures and compositions, the amount and composition of phases in an alloy at a given temperature, the amount of a certain phase in different steels, and the microstructure developed in different alloys.