Abstract
Quantitative image analysis has expanded the capabilities of surface analysis significantly with the use of computer technology. This article provides an overview of the quantitative image analysis and optical microscopy. It describes the various steps involved in surface preparation of samples prone to abrasion damage and artifacts for quantitative image analysis.
You do not currently have access to this chapter.
Citation
Donald C. Zipperian, Microstructural Analysis of Finished Surfaces, Surface Engineering, Vol 5, ASM Handbook, Edited By C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr., ASM International, 1994, p 139–143, https://doi.org/10.31399/asm.hb.v05.a0001237
Download citation file:
Related Book Content
Mechanical Grinding and Polishing
Metallography and Microstructures
X-Ray Photoelectron Spectroscopy
Materials Characterization
Particle Size and Size Distribution
Powder Metallurgy
Auger Electron Spectroscopy
Materials Characterization (2019 Edition)
Thermal Desorption Spectroscopy
Materials Characterization (2019 Edition)
Surface Finishing
Stainless Steels for Design Engineers
Raman Spectroscopy
Materials Characterization
X-Ray Photoelectron Spectroscopy
Materials Characterization (2019 Edition)
Rutherford Backscattering Spectrometry
Materials Characterization
Introduction to Surface Analysis
Materials Characterization (2019 Edition)