Resonant Ultrasound Spectroscopy Testing Methods in Additive Manufacturing
-
Published:2023
Abstract
This article presents the basic principle, characteristics, advantages, and disadvantages of resonant ultrasound spectroscopy (RUS) methods in additive manufacturing. It focuses on the two types of RUS methods: the swept-sine method and the impulse excitation method. Representative significant results for additively manufactured complex parts obtained with the different RUS systems are also shown. The article also presents the basic principle and examples of nonlinear RUS methods.
Anne-Françoise Obaton, Resonant Ultrasound Spectroscopy Testing Methods in Additive Manufacturing, Additive Manufacturing Design and Applications, Vol 24A, ASM Handbook, Edited By Mohsen Seifi, David L. Bourell, William Frazier, Howard Kuhn, ASM International, 2023, p 1–12, https://doi.org/10.31399/asm.hb.v24A.a0006953
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.